Dual‐Phase Ligand Engineering Enables 18.21% FAPbI 3 Quantum Dot Solar Cells
Advanced Materials · 2025-02 · 37 (8)
DOI: 10.1002/adma.202417346 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 05.01.2025. Verfasst von Du Li und 7 weiteren Autor:innen. Beteiligte Einrichtung: Institute of Functional Nano & Soft Materials (FUNSOM), Jiangsu Key Laboratory of Advanced Negative Carbon Technologies, Soochow University, 199 Ren-…. Die Arbeit wurde bisher 37-mal zitiert (Crossref) und nennt 46 Literaturangaben. Gefördert von: National Key Research and Development Program of China, National Natural Science Foundation of China, China National Postdoctoral Program for Innovative Talents.
Abstract (Originalsprache)
Formamidinium lead triiodide (FAPbI 3 ) perovskite quantum dot (PQD) are promising candidate for high‐performing quantum dot photovoltaic due to its narrow bandgap, high ambient stability, and long carrier lifetime. However, the carrier transport blockage and nonradiative recombination loss, originating from the high‐dielectric ligands and defects/trap states on the FAPbI 3 PQD surface, significantly limit the efficiency and stability of its photovoltaic performance. In this work, through exploring dual‐site molecular ligands, namely 2‐thiophenemethylammonium iodide (2‐TM) and 2‐thiopheneethylammonium iodide (2‐TE), a dual‐phase synergistic ligand exchange (DSLE) protocol consisting of both solution‐phase and solid‐state ligand engineering is demonstrated. The DSLE strategy effectively replaces the native long insulating ligands and simultaneously passivate surface defects in hybrid FAPbI 3 PQDs, leading to enhanced electronic coupling for efficient charge transport. Consequently, the FAPbI 3 PQD solar cell based on DSLE strategy achieves a notable enhanced efficiency from 15.43% to 17.79% (2‐TM) and 18.21% (2‐TE), respectively. Besides, both 2‐TM and 2‐TE engineered devices exhibit enhanced stability, maintaining over 80% of its initial efficiency after aging in ambient environment (20–30% humidity, 25 °C) for over 1400 h. It believes these findings will provide a new protocol to precisely regulate the surface chemistry of hybrid PQDs toward high‐performance optoelectronic applications.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Institute of Functional Nano & Soft Materials (FUNSOM), Jiangsu Key Laboratory of Advanced Negative Carbon Technologies, Soochow University, 199 Ren-Ai Road, Suzhou Industrial Park, Suzhou, Jiangsu, 215123, P. R. China.
- Jiangsu Key Laboratory of Micro and Nano Heat Fluid Flow Technology and Energy Application, School of Physical Science and Technology, Suzhou University of Science and Technology, Suzhou, Jiangsu, 215009, P. R. China.
ORCID-Profile: Jianyu Yuan
Förderung
- National Key Research and Development Program of China
- National Natural Science Foundation of China
- China National Postdoctoral Program for Innovative Talents
- China Postdoctoral Science Foundation
- Natural Science Foundation of Jiangsu Province
Zitieren
APA
Li, D., Zhao, C., Zhang, X., Zhao, X., Huang, H., Li, H., Li, F., & Yuan, J. (2025). Dual‐Phase Ligand Engineering Enables 18.21% FAPbI 3 Quantum Dot Solar Cells. Advanced Materials, 37(8). https://doi.org/10.1002/adma.202417346
Vancouver
Li D, Zhao C, Zhang X, Zhao X, Huang H, Li H, et al. Dual‐Phase Ligand Engineering Enables 18.21% FAPbI 3 Quantum Dot Solar Cells. Advanced Materials. 2025;37(8). doi:10.1002/adma.202417346
BibTeX
@article{Li2025,
author = {Li, Du and Zhao, Chenyu and Zhang, Xuliang and Zhao, Xinyu and Huang, Hehe and Li, Huifeng and Li, Fangchao and Yuan, Jianyu},
title = {Dual‐Phase Ligand Engineering Enables 18.21% FAPbI 3 Quantum Dot Solar Cells},
journal = {Advanced Materials},
year = {2025},
volume = {37},
number = {8},
doi = {10.1002/adma.202417346}
}
EUVIMED