Selenium‐Anchored Chlorine Redox Chemistry in Aqueous Zinc Dual‐Ion Batteries

Ze Chen, Yue Hou, Yiqiao Wang, Zhiquan Wei, Ao Chen, Pei Li, Zhaodong Huang, Nan Li, Chunyi Zhi iD

Advanced Materials · 2024-02 · 36 (6)

DOI: 10.1002/adma.202309330 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 06.12.2023. Verfasst von Ze Chen und 8 weiteren Autor:innen. Beteiligte Einrichtung: Department of Materials Science and Engineering, City University of Hong Kong, 83 Tat Chee Avenue, Kowloon, Hong Kong, 999077, China. Die Arbeit wurde bisher 33-mal zitiert (Crossref) und nennt 56 Literaturangaben. Gefördert von: National Key Research and Development Program of China, RGC Collaborative Research Fund, Science and Technology Planning Project of Shenzen Municipality.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Chlorine‐based batteries with Cl 0 to Cl − redox reaction (ClRR) are promising for high‐performance energystorage due to their high redox potential and large theoretical capacity. However, the inherent gas–liquid conversion feature of ClRR together with poor Cl fixation can cause Cl 2 leakage, reducing battery reversibility. Herein, we utilize a Se‐based organic molecule, diphenyl diselenide ( di ‐Ph‐Se), as the Cl anchoring agent and realize an atomic level‐Cl fixation through chalcogen‐halogencoordinating chemistry. The promoted Cl fixation, with two oxidized Cl 0 anchoring on a single Ph‐Se, and the multivalence conversion of Se contributeto a six‐electron conversion process with up to 507 mAh g −1 and an average voltage of 1.51 V, as well as a high energy density of 665 Wh Kg −1 . Based on the superior reversibility of thedeveloped di ‐Ph‐Se electrode with ClRR, a remarkable rate performance (205 mAh g −1 at 5 A g −1 ) and cycling performance (capacity retention of 77.3 % after 500cycles) are achieved. Significantly, the pouch cell delivers a record arealcapacity of up to 6.87 mAh cm −2 and extraordinary self‐discharge performance. This chalcogen‐halogen coordination chemistry between the Se electrode and Cl provides a new insight for developing reversible and efficientbatteries with halogen redox reactions.

Schlagwörter

Stichwörter der Autor:innen

aqueous batteriesorganic electrodeszinc batterieszinc-ion batteries

Autor:innen und Institutionen

  • Department of Materials Science and Engineering, City University of Hong Kong, 83 Tat Chee Avenue, Kowloon, Hong Kong, 999077, China.
  • Hong Kong Center for Cerebro-Cardiovascular Health Engineering (COCHE), NT, HKSAR, Shatin, 999077, China.
  • CityU-Matter Science Research Institute, Shenzhen, 518000, China.

ORCID-Profile: Chunyi Zhi

Förderung

  • National Key Research and Development Program of China
  • RGC Collaborative Research Fund
  • Science and Technology Planning Project of Shenzen Municipality

Zitieren

APA

Chen, Z., Hou, Y., Wang, Y., Wei, Z., Chen, A., Li, P., Huang, Z., Li, N., & Zhi, C. (2024). Selenium‐Anchored Chlorine Redox Chemistry in Aqueous Zinc Dual‐Ion Batteries. Advanced Materials, 36(6). https://doi.org/10.1002/adma.202309330

Vancouver

Chen Z, Hou Y, Wang Y, Wei Z, Chen A, Li P, et al. Selenium‐Anchored Chlorine Redox Chemistry in Aqueous Zinc Dual‐Ion Batteries. Advanced Materials. 2024;36(6). doi:10.1002/adma.202309330

BibTeX
@article{Chen2024,
  author = {Chen, Ze and Hou, Yue and Wang, Yiqiao and Wei, Zhiquan and Chen, Ao and Li, Pei and Huang, Zhaodong and Li, Nan and Zhi, Chunyi},
  title = {Selenium‐Anchored Chlorine Redox Chemistry in Aqueous Zinc Dual‐Ion Batteries},
  journal = {Advanced Materials},
  year = {2024},
  volume = {36},
  number = {6},
  doi = {10.1002/adma.202309330}
}
Kostenlos starten →