EUVIMEDEUVIMED entdecken
Crossref

Fluorinating All Interfaces Enables Super‐Stable Solid‐State Lithium Batteries by In Situ Conversion of Detrimental Surface Li 2 CO 3

Yong Guo, Siyuan Pan, Xuerui Yi, Sijia Chi, Xunjie Yin, Chuannan Geng, Qianhui Yin, QinYi Zhan, Ziyun Zhao, Feng-Min Jin, Hui Fang, Yan-Bing He iD und 3 weitere

Advanced Materials · 2024-03 · 36 (13)

DOI: 10.1002/adma.202308493 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Materials, online erschienen am 28.12.2023. Verfasst von Yong Guo und 14 weiteren Autor:innen. Beteiligte Einrichtung: Nanoyang Group, Tianjin Key Laboratory of Advanced Carbon and Electrochemical Energy Storage, School of Chemical Engineering and Technology, and Coll…. Die Arbeit wurde bisher 87-mal zitiert (Crossref) und nennt 58 Literaturangaben. Gefördert von: National Key Research and Development Program of China, National Natural Science Foundation of China, Haihe Laboratory of Sustainable Chemical Transformations.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Li‐stuffed battery materials intrinsically have surface impurities, typically Li 2 CO 3 , which introduce severe kinetic barriers and electrochemical decay for a cycling battery. For energy‐dense solid‐state lithium batteries (SSLBs), mitigating detrimental Li 2 CO 3 from both cathode and electrolyte materials is required, while the direct removal approaches hardly avoid Li 2 CO 3 regeneration. Here, a decarbonization–fluorination strategy to construct ultrastable LiF‐rich interphases throughout the SSLBs by in situ reacting Li 2 CO 3 with LiPF 6 at 60 °C is reported. The fluorination of all interfaces effectively suppresses parasitic reactions while substantially reducing the interface resistance, producing a dendrite‐free Li anode with an impressive cycling stability of up to 7000 h. Particularly, transition metal dissolution associated with gas evolution in the cathodes is remarkably reduced, leading to notable improvements in battery rate capability and cyclability at a high voltage of 4.5 V. This all‐in‐one approach propels the development of SSLBs by overcoming the limitations associated with surface impurities and interfacial challenges.

Schlagwörter

Stichwörter der Autor:innen

LiF‐rich interphasesdecarbonization–fluorinationgarnetsolid‐state lithium batteriessurface impurities

Autor:innen und Institutionen

  • Nanoyang Group, Tianjin Key Laboratory of Advanced Carbon and Electrochemical Energy Storage, School of Chemical Engineering and Technology, and Collaborative Innovation Center of Chemical Science and Engineering (Tianj…
  • National Industry-Education Integration Platform of Energy Storage, Tianjin University, Tianjin, 300072, China.
  • Haihe Laboratory of Sustainable Chemical Transformations, Tianjin, 300192, China.
  • Shenzhen Geim Graphene Center, Institute of Materials Research (IMR), Tsinghua Shenzhen International Graduate School, Tsinghua University, Shenzhen, 518055, China.
  • Joint School of National University of Singapore and Tianjin University, International Campus of Tianjin University, Fuzhou, 350207, China.

ORCID-Profile: Yan-Bing He, Quan-Hong Yang

Förderung

  • National Key Research and Development Program of China
  • National Natural Science Foundation of China
  • Haihe Laboratory of Sustainable Chemical Transformations
  • Fundamental Research Funds for the Central Universities

Zitieren

APA

Guo, Y., Pan, S., Yi, X., Chi, S., Yin, X., Geng, C., Yin, Q., Zhan, Q., Zhao, Z., Jin, F. M., Fang, H., He, Y. B., Kang, F., Wu, S., & Yang, Q. H. (2024). Fluorinating All Interfaces Enables Super‐Stable Solid‐State Lithium Batteries by In Situ Conversion of Detrimental Surface Li 2 CO 3. Advanced Materials, 36(13). https://doi.org/10.1002/adma.202308493

Vancouver

Guo Y, Pan S, Yi X, Chi S, Yin X, Geng C, et al. Fluorinating All Interfaces Enables Super‐Stable Solid‐State Lithium Batteries by In Situ Conversion of Detrimental Surface Li 2 CO 3. Advanced Materials. 2024;36(13). doi:10.1002/adma.202308493

BibTeX
@article{Guo2024,
  author = {Guo, Yong and Pan, Siyuan and Yi, Xuerui and Chi, Sijia and Yin, Xunjie and Geng, Chuannan and Yin, Qianhui and Zhan, QinYi and Zhao, Ziyun and Jin, Feng-Min and Fang, Hui and He, Yan-Bing and Kang, Feiyu and Wu, Shichao and Yang, Quan-Hong},
  title = {Fluorinating All Interfaces Enables Super‐Stable Solid‐State Lithium Batteries by In Situ Conversion of Detrimental Surface Li 2 CO 3},
  journal = {Advanced Materials},
  year = {2024},
  volume = {36},
  number = {13},
  doi = {10.1002/adma.202308493}
}
Kostenlos starten →