Residual LiF‐Derived Interfacial Engineering Enables Stable SiO x /Spent Graphite Anodes With Fast Li + Transport and Superior Interfacial Stability
Advanced Functional Materials · 20.11.2026
DOI: 10.1002/adfm.79741 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Functional Materials, online erschienen am 20.11.2026. Verfasst von Tiefei Li und 10 weiteren Autor:innen. Die Arbeit nennt 50 Literaturangaben.
Abstract (Originalsprache)
Although SiO x /graphite composite anodes can mitigate SiO x volume expansion and poor electronic conductivity, loose physical contact between both phases leads to suboptimal performance. Meanwhile, large‐scale disposal of spent graphite (SG) remains a challenge. SG contains residual LiF and LiF‐derived solid electrolyte interphase (SEI) components. Herein, we propose integrating SG with SiO x via mechanical ball milling. Mechanical forces roughen SiO x surfaces and embed LiF, distributing lithiation and delithiation stresses, minimizing volume mismatch with graphite layers, and promoting intimate contact. An optimal SiO x ‐to‐SG mass ratio of 8:2 ensures capacity and electrochemical performance. LiF modulates interfacial side reactions, absorbs mechanical stress, harmonizes interfacial electronic structures, and enhances Li + diffusion kinetics and structural stability. The SiO x /SG half‐cell with 2 wt.% LiF delivers 766.8 mAh g −1 at 2 C and retains 921.4 mAh g −1 after 200 cycles at 400 mA g −1 (80.1% capacity retention). The full cell paired with NCM811 also exhibits improved cycling stability. Further FEC‐free tests support a beneficial role of pre‐introduced LiF in interfacial impedance evolution, Li + diffusion kinetics, and cycling performance. Applicable to diverse SG types, this study highlights a sustainable interfacial engineering strategy for high‐value SG recycling and durable high‐capacity SiO x anodes, offering economic and environmental benefits.
Zitieren
APA
Li, T., Hou, J., Liang, Y., Yang, W., Tan, M., Ma, S., Li, L., Li, X., Yang, H., Zhang, Y., & Zhang, Y. (2026). Residual LiF‐Derived Interfacial Engineering Enables Stable SiO x /Spent Graphite Anodes With Fast Li + Transport and Superior Interfacial Stability. Advanced Functional Materials. https://doi.org/10.1002/adfm.79741
Vancouver
Li T, Hou J, Liang Y, Yang W, Tan M, Ma S, et al. Residual LiF‐Derived Interfacial Engineering Enables Stable SiO x /Spent Graphite Anodes With Fast Li + Transport and Superior Interfacial Stability. Advanced Functional Materials. 2026. doi:10.1002/adfm.79741
BibTeX
@article{Li2026,
author = {Li, Tiefei and Hou, Jiyue and Liang, Yongshun and Yang, Wenhao and Tan, Mao and Ma, Shichao and Li, Lei and Li, Xue and Yang, Haoqi and Zhang, Yingjie and Zhang, Yiyong},
title = {Residual LiF‐Derived Interfacial Engineering Enables Stable SiO x /Spent Graphite Anodes With Fast Li + Transport and Superior Interfacial Stability},
journal = {Advanced Functional Materials},
year = {2026},
doi = {10.1002/adfm.79741}
}
EUVIMED