Concentration‐Dependent Li‐Ion Solvation and Dual‐Interphase Regulation by Cyanuric Chloride in Lithium‐Sulfur Batteries
Advanced Functional Materials · 20.11.2026
DOI: 10.1002/adfm.79722 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Functional Materials, online erschienen am 20.11.2026. Verfasst von Ryanda Enggar Anugrah Ardhi und 9 weiteren Autor:innen. Die Arbeit nennt 78 Literaturangaben. Gefördert von: Ministry of Science and ICT, South Korea, National Research Foundation of Korea.
Abstract (Originalsprache)
Practical lithium‐sulfur (Li‐S) batteries require control of dissolved polysulfides, sulfur‐conversion kinetics, and lithium‐metal anodes under high sulfur loading and limited electrolyte. Dissolved molecular additives can influence all three processes, but their effects depend on concentration. Here, cyanuric chloride (CC) is examined from 0 to 0.10 M as an aprotic chlorotriazine additive with three ring‐nitrogen sites and three carbon‐chlorine centers. Spectroscopy suggests that 0.05 M (Optm‐CC) enhances nitrate (NO 3 − ) and bis(trifluoromethanesulfonyl)imide (TFSI − ) anions’ participation in Li‐ion solvation. This concentration reduces polysulfide crossover, enriches the sulfur‐cathode interphase with inorganic and triazine‐associated products, and promotes an inorganic‐rich, Cl‐containing interphase at the lithium‐metal anode. As a result, these changes lower cyclic‐voltammetry peak separation to 0.191 V, raise the apparent Li|Li exchange‐current density to 0.203 mA cm −2 , support Li|Li symmetric‐cell cycling for over 1100 cycles, deliver 560 mAh g Sulfur −1 at 10C, and sustain 3000 Li‐S cycles. Increasing the CC concentration to 0.10 M (Conc‐CC) produces a larger spectroscopic shift, but the apparent Li‐ion transference number and lithium‐electrode polarization deteriorate. Furthermore, a pouch cell operated at 8 mg Sulfur cm −2 and 5 µL mg Sulfur − 1 retains 72.73% of its stabilized capacity after 300 cycles. Among the tested formulations, 0.05 M best balances coordination, interphase chemistry, and electrochemical performance.
Förderung
- Ministry of Science and ICT, South Korea
- National Research Foundation of Korea
Zitieren
APA
Ardhi, R. E. A., Konavarapu, S. K., Elli, F. H., Ha, J., Soundararajan, V., Yoo, H., Kim, H., Subiyanto, I., Kim, J. W., & Oh, I. (2026). Concentration‐Dependent Li‐Ion Solvation and Dual‐Interphase Regulation by Cyanuric Chloride in Lithium‐Sulfur Batteries. Advanced Functional Materials. https://doi.org/10.1002/adfm.79722
Vancouver
Ardhi REA, Konavarapu SK, Elli FH, Ha J, Soundararajan V, Yoo H, et al. Concentration‐Dependent Li‐Ion Solvation and Dual‐Interphase Regulation by Cyanuric Chloride in Lithium‐Sulfur Batteries. Advanced Functional Materials. 2026. doi:10.1002/adfm.79722
BibTeX
@article{Ardhi2026,
author = {Ardhi, Ryanda Enggar Anugrah and Konavarapu, Satyanarayana K. and Elli, Farris Hilmyafif and Ha, Jawon and Soundararajan, Vidhurathan and Yoo, Hyunjoon and Kim, Hyunsoo and Subiyanto, Iyan and Kim, Jeong Won and Oh, Il‐Kwon},
title = {Concentration‐Dependent Li‐Ion Solvation and Dual‐Interphase Regulation by Cyanuric Chloride in Lithium‐Sulfur Batteries},
journal = {Advanced Functional Materials},
year = {2026},
doi = {10.1002/adfm.79722}
}
EUVIMED