Catalyst‐Mediated Interfacial Prelithiation for Energy/Power‐Dense and Ultralong‐Life Lithium Batteries
Advanced Functional Materials · 2026-07 · 36 (61)
DOI: 10.1002/adfm.76790 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Functional Materials, online erschienen am 07.07.2026. Verfasst von Ahu Shao und 9 weiteren Autor:innen. Die Arbeit nennt 49 Literaturangaben. Gefördert von: National Natural Science Foundation of China.
Abstract (Originalsprache)
The irreversible cation depletion and interfacial degradation fundamentally limit the practical energy output and cycling endurance of lithium‐free anode batteries. Here, we propose a catalyst‐mediated interfacial prelithiation strategy that offsets irreversible lithium loss, precisely optimizes Li + kinetics and interfacial stability for energy/power‐dense cell prototypes. The sulfurized polyacrylonitrile (SPAN) catalyst, featuring electron‐withdrawing sulfur sites, facilitates C‐C bond cleavage through S‐Li interactions. The Li 2 C 2 O 4 @SPAN composite delivers a delithiation voltage of 3.90 V and a highly efficient Li utilization of 99.5%. When paired with the LiNi 0.8 Co 0.1 Mn 0.1 O 2 cathode, the prelithiation layer achieves Li + replenishment areal capacities up to 1.1 mAh cm −2 . Furthermore, the bilayer configuration spatially isolates prelithiation agents from the cathode's redox center, alleviating the gas‐induced structural collapse and stress accumulation. Meanwhile, the SPAN‐derived ROSO 3 Li species form a robust cathode interphase with LiF domains, accelerating Li + transport and stabilizing the 4.5 V charging process. Under the lean‐electrolyte condition (1.7 g Ah −1 ) in 1.28 Ah pouch cells, the Cu||NCM811‐LS prototype achieves gravimetric/volumetric energy densities of 460 Wh kg −1 /1083 Wh L −1 and a peak power output of 858 W kg −1 . In addition, a 2.8 Ah Gr||NCM811 cell incorporating this prelithiation reservoir maintains a capacity retention of 88.2% over 1000 cycles. As a “drop‐in” solution requiring no changes to cell assembly, this interfacial prelithiation paradigm aligns with scalable industrial manufacturing, affording a readily adoptable path toward energy/power‐dense lithium batteries.
Förderung
- National Natural Science Foundation of China
Zitieren
APA
Shao, A., Li, C., Liu, J., Wang, Z., Jia, Q., Wang, X., Wang, Z., Wang, J., Xu, F., & Ma, Y. (2026). Catalyst‐Mediated Interfacial Prelithiation for Energy/Power‐Dense and Ultralong‐Life Lithium Batteries. Advanced Functional Materials, 36(61). https://doi.org/10.1002/adfm.76790
Vancouver
Shao A, Li C, Liu J, Wang Z, Jia Q, Wang X, et al. Catalyst‐Mediated Interfacial Prelithiation for Energy/Power‐Dense and Ultralong‐Life Lithium Batteries. Advanced Functional Materials. 2026;36(61). doi:10.1002/adfm.76790
BibTeX
@article{Shao2026,
author = {Shao, Ahu and Li, Chunwei and Liu, Jiacheng and Wang, Zhiqiao and Jia, Qiurong and Wang, Xin and Wang, Zhaohui and Wang, Jiangan and Xu, Fei and Ma, Yue},
title = {Catalyst‐Mediated Interfacial Prelithiation for Energy/Power‐Dense and Ultralong‐Life Lithium Batteries},
journal = {Advanced Functional Materials},
year = {2026},
volume = {36},
number = {61},
doi = {10.1002/adfm.76790}
}
EUVIMED