Deciphering Solid‐State Battery Interface Failure: Plasma‐Assisted Bulk‐Interface Lithium Diffusion Kinetics Regulation
Advanced Functional Materials · 2026-03 · 36 (19)
DOI: 10.1002/adfm.202521740 ↗Kurz gefasst
Fachartikel in der Zeitschrift Advanced Functional Materials, online erschienen am 16.10.2025. Verfasst von Jialong Wu und 7 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 48 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Basic and Applied Basic Research Foundation of Guangdong Province, Zhejiang Provincial Outstanding Youth Science Foundation.
Abstract (Originalsprache)
Interfacial‐contact failure and void‐evolution in garnet‐based solid‐state lithium‐metal batteries (SSLMBs), caused by inadequate initial interface‐bonding and limited lithium‐ion diffusion at the anode, represent critical bottlenecks that need to be addressed to achieve the practical viability of SSLMBs. Here, a plasma‐assisted dual‐strategy is presented that integrates radio‐frequency plasma‐magnetron‐sputtering (RF‐PMS) and dielectric‐barrier‐discharge (DBD) plasma‐treatment to construct an outstanding interface structure. Specifically, the composite‐lithium‐anode (CLA) doped with DBD plasma‐functionalized carbon‐nanotubes (D‐CNT) is coated onto an AlF 3 ‐modified Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 (AF‐LLZTO) solid electrolyte synthesized using RF‐PMS. The engineered LC10|AF‐LLZTO interface (LC10: optimized CLA containing 10 wt.% D‐CNT) facilitates a stable lithium‐ion diffusion pathway, effectively mitigating interfacial‐contact degradation. Following delithiation to 3.0 mAh cm −2 , this configuration retains 85.16% interfacial‐contact integrity—significantly surpassing the mere 10.49% retention observed in unmodified lithium‐anodes. The enhanced interfacial‐stability of this structure can be directly visualized through in situ optical‐microscopy observation. The symmetric cell LC10|AF‐LLZTO‐AF|LC10 achieves 10000 h of stable cycling at 0.2 mA cm −2 , significantly outperforming the symmetric cells Li|AF‐LLZTO‐AF|Li without CLA (1930 h) and LC10|LLZTO|LC10 without AlF 3 (
Förderung
- National Natural Science Foundation of China
- Basic and Applied Basic Research Foundation of Guangdong Province
- Zhejiang Provincial Outstanding Youth Science Foundation
Zitieren
APA
Wu, J., Chen, W., Hao, B., Wang, Y., Xu, Z., Wang, Q., Jiang, Z., & Jiang, Z. (2026). Deciphering Solid‐State Battery Interface Failure: Plasma‐Assisted Bulk‐Interface Lithium Diffusion Kinetics Regulation. Advanced Functional Materials, 36(19). https://doi.org/10.1002/adfm.202521740
Vancouver
Wu J, Chen W, Hao B, Wang Y, Xu Z, Wang Q, et al. Deciphering Solid‐State Battery Interface Failure: Plasma‐Assisted Bulk‐Interface Lithium Diffusion Kinetics Regulation. Advanced Functional Materials. 2026;36(19). doi:10.1002/adfm.202521740
BibTeX
@article{Wu2026,
author = {Wu, Jialong and Chen, Weiheng and Hao, Bin and Wang, Yichun and Xu, Zejun and Wang, Qiushi and Jiang, Zhong‐Jie and Jiang, Zhongqing},
title = {Deciphering Solid‐State Battery Interface Failure: Plasma‐Assisted Bulk‐Interface Lithium Diffusion Kinetics Regulation},
journal = {Advanced Functional Materials},
year = {2026},
volume = {36},
number = {19},
doi = {10.1002/adfm.202521740}
}
EUVIMED