EUVIMEDEUVIMED entdecken
Crossref

Doping‐Induced Ultrafast Kinetics of Na 4 Fe 3 (PO 4 ) 2 P 2 O 7 Cathode Enabling Wide Temperature Sodium‐Ion Battery

Shiyu Wang, Qiao Zhang, Haiyun Zhu, Yuanyuan Du, Kai Yu, Dong Zhou, Yonghong Deng, Jun Wang, Jikang Jian

Advanced Functional Materials · 2026-04 · 36 (29)

DOI: 10.1002/adfm.202520871 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Functional Materials, online erschienen am 06.12.2025. Verfasst von Shiyu Wang und 8 weiteren Autor:innen. Die Arbeit wurde bisher 15-mal zitiert (Crossref) und nennt 48 Literaturangaben. Gefördert von: National Natural Science Foundation of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Na 4 Fe 3 (PO 4 ) 2 P 2 O 7 (NFPP) is a promising cathode material for sodium‐ion batteries (SIBs) because of its low cost and relatively stable cycling performance. However, NFPP behaves neither satisfied rate capability at low temperature nor long‐term stable cycling performance at high temperature due to its inherent low conductivity and structural degradations upon cycling, which hinders its broad applications under extreme conditions. Herein, a wide‐temperature Na 3.96 K 0.04 Fe 3 (PO 4 ) 2 P 2 O 7 (NKFPP) is developed via a small amount of K doping. The doping not only reduces the migration energy barrier of Na + , but also inhibits structural rearrangement and anion cluster deformation during the desodiation from the Na1 and Na4 sites, which are verified by comprehensive characterizations. As a result, the obtained NKFPP has a discharge capacity of 87.1 mAh g −1 at 40C (1C = 129 mA g −1 ) and 30 °C, and maintains 75.41% capacity retention for 10 000 cycles. Even at 10C and 60 °C, the NKFPP delivers a high discharge capacity of 94.3 mAh g −1 with capacity retention of 90.12% for 1000 cycles. Moreover, the K‐doped NFPP exhibits obviously better rate capability than the undoped sample at −20 °C. Therefore, this work provides guidance for further research and development of high‐performance, wide‐temperature‐range polyanion phosphate cathode materials.

Förderung

  • National Natural Science Foundation of China

Zitieren

APA

Wang, S., Zhang, Q., Zhu, H., Du, Y., Yu, K., Zhou, D., Deng, Y., Wang, J., & Jian, J. (2026). Doping‐Induced Ultrafast Kinetics of Na 4 Fe 3 (PO 4 ) 2 P 2 O 7 Cathode Enabling Wide Temperature Sodium‐Ion Battery. Advanced Functional Materials, 36(29). https://doi.org/10.1002/adfm.202520871

Vancouver

Wang S, Zhang Q, Zhu H, Du Y, Yu K, Zhou D, et al. Doping‐Induced Ultrafast Kinetics of Na 4 Fe 3 (PO 4 ) 2 P 2 O 7 Cathode Enabling Wide Temperature Sodium‐Ion Battery. Advanced Functional Materials. 2026;36(29). doi:10.1002/adfm.202520871

BibTeX
@article{Wang2026,
  author = {Wang, Shiyu and Zhang, Qiao and Zhu, Haiyun and Du, Yuanyuan and Yu, Kai and Zhou, Dong and Deng, Yonghong and Wang, Jun and Jian, Jikang},
  title = {Doping‐Induced Ultrafast Kinetics of Na 4 Fe 3 (PO 4 ) 2 P 2 O 7 Cathode Enabling Wide Temperature Sodium‐Ion Battery},
  journal = {Advanced Functional Materials},
  year = {2026},
  volume = {36},
  number = {29},
  doi = {10.1002/adfm.202520871}
}
Kostenlos starten →