Microstructural Evolution and Mechanical Property Degradation of Sn0.5Ag0.7Cu5Bi Solder Joints with High Indium Alloying

Liuwei Wang, Huidong Gu, Xiaojing Wang, Shanshan Cai, Saad Alshammari, Gaber A. M. Mersal, Yanlai Wang, Xulei Wu, Hanhui Lei, Juanna Ren, Mohamed M. Ibrahim, Terence X. Liu

Advanced Engineering Materials · 2025-11 · 27 (21)

DOI: 10.1002/adem.202500843 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Advanced Engineering Materials, online erschienen am 04.10.2025. Verfasst von Liuwei Wang und 11 weiteren Autor:innen. Die Arbeit wurde bisher 6-mal zitiert (Crossref) und nennt 63 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

This study systematically investigates the effects of indium (In) addition (4–17 wt%) on Sn0.5Ag0.7Cu5Bi solder joints through thermal analysis, microstructural characterization, and mechanical testing. Key findings reveal that 12 wt% In emerges as the optimal composition, offering superior mechanical performance with 87% ductile fracture and significantly suppressed intermetallic compound (IMC) growth. However, high‐In alloys (15–17 wt%) exhibit abnormal IMC thickening due to thermal activation near the aging temperature. Microstructural analysis suggests that In substitution at Sn sites causes the lattice to induce the aging local lattice contraction in η ′‐Cu 6 Sn 5 , generating internal stresses that lead to cracking in low‐In alloys after prolonged aging. Shear strength shows a nonmonotonic dependence on In content, decreasing as In increases, attributed to InSn 4 phase formation. This research identifies 12 wt% In as the optimal composition for Sn0.5Ag0.7Cu5Bi‐xIn solders, providing specific design rules for industrial applications: 1) enhanced drop resistance in mobile devices due to 87% ductile fracture; 2) cost reduction in automotive electronics by suppressing IMC growth (81% thickness reduction vs. 4In alloy); and 3) compatibility with flexible substrates via In‐induced lattice contraction, validated by density functional theory calculations. These guidelines enable reliable solder joints in high‐density IC packaging under thermal cycling.

Zitieren

APA

Wang, L., Gu, H., Wang, X., Cai, S., Alshammari, S., Mersal, G. A. M., Wang, Y., Wu, X., Lei, H., Ren, J., Ibrahim, M. M., & Liu, T. X. (2025). Microstructural Evolution and Mechanical Property Degradation of Sn0.5Ag0.7Cu5Bi Solder Joints with High Indium Alloying. Advanced Engineering Materials, 27(21). https://doi.org/10.1002/adem.202500843

Vancouver

Wang L, Gu H, Wang X, Cai S, Alshammari S, Mersal GAM, et al. Microstructural Evolution and Mechanical Property Degradation of Sn0.5Ag0.7Cu5Bi Solder Joints with High Indium Alloying. Advanced Engineering Materials. 2025;27(21). doi:10.1002/adem.202500843

BibTeX
@article{Wang2025,
  author = {Wang, Liuwei and Gu, Huidong and Wang, Xiaojing and Cai, Shanshan and Alshammari, Saad and Mersal, Gaber A. M. and Wang, Yanlai and Wu, Xulei and Lei, Hanhui and Ren, Juanna and Ibrahim, Mohamed M. and Liu, Terence X.},
  title = {Microstructural Evolution and Mechanical Property Degradation of Sn0.5Ag0.7Cu5Bi Solder Joints with High Indium Alloying},
  journal = {Advanced Engineering Materials},
  year = {2025},
  volume = {27},
  number = {21},
  doi = {10.1002/adem.202500843}
}
Kostenlos starten →